I had some severe delamination a.k.a layer separation but specifically on the top layer
The slicer’s profile for my printer set top-level speed to 200 mm/s so I halved it, and now there’s almost no delamination at all
I had some severe delamination a.k.a layer separation but specifically on the top layer
The slicer’s profile for my printer set top-level speed to 200 mm/s so I halved it, and now there’s almost no delamination at all
Lower speed means less flow through the nozzle and warmer plastic. It will have more time at the melting temperature and therefore stick better to the previous layer.