This is layer 2 or 3. It will be covered by the next few layers but I feel like it shouldn’t be this fugly. I’m using Cura’s Standard Quality except for temp which is set to 205. The filament is Inland PLA.
This is layer 2 or 3. It will be covered by the next few layers but I feel like it shouldn’t be this fugly. I’m using Cura’s Standard Quality except for temp which is set to 205. The filament is Inland PLA.
Yeah, that looks much better. Do you have a self leveling bed? If your bed has a high point that is not captured in its measurements its possible that your still getting just a bit more drag in that specific spot.
One thing you can do to test, is to move the print to a different spot on the bed in your slicer.