I’ve mostly gotten the quality to where I’m happy except for whatever it’s doing to the bow of Benchy. Still some stringing but I don’t expect that to go away completely with TPU. Hatchbox TPU, been lowering temp, lowering print speed, fine tuning retraction, etc. I can give exact numbers if needed, but if anyone knows what to adjust specifically for what it’s doing at the bow that would be great.

  • morbidcactus@lemmy.ca
    link
    fedilink
    English
    arrow-up
    1
    ·
    7 days ago

    It’ll cause more zits and the like, more stringing, don’t know that’d 100% cause the issue but certainly won’t help.

    I just did a round of nylon last week which is also super hygroscopic, bag’s like at most 8 months old but seal was intact. Even printing out of a drybox with fresh desiccant I noticed more stringing and occasional blobs + nozzle buildup over the few days (Was redoing my hotend so I inspected it, no sign of nozzle leaking), can definitely make overhangs worse.